The air file is followed by 80-grit, and then 180-grit on a long board by hand. This eliminates the deep sanding scratches that can resurface later in the paint as the topcoat and primers shrink back. Although the entire repair area is coated in filler, it is paper thin, actually no thicker than the old paint in most areas. View Related Article
|
|